Daiwa Fine Chemicals Co., Ltd. Official site

Low-foam neutral tin plating DAIN TINGOOD 314

This is a neutral tin plating process for barrels with low foaming and a pH of 7.

■ DAIN TINGOOD 314 bath has a pH of 7, so it does not damage materials such as ceramic chips. ■ It has almost zero foaming and excellent plating workability. ■ It suppresses the generation of precipitates from tetravalent tin and has excellent bath stability.

Related Link - https://www.daiwafc.co.jp/metal/865

basic information

■ Bath temperature: 30 ℃ ■ pH=7 ■ Current density: Usable at 0.5 to 2.0 A/dm²

Price range

Delivery Time

Applications/Examples of results

Ceramics chip components, such as electrode formation.

Low-foaming neutral tin plating DAIN TINGOOD 314

PRODUCT

Recommended products

Distributors

"Things that no one has done yet" and "There are surely people who will be happy if it exists"… The Yamato Kasei Group develops its unique chemical business in niche markets that major manufacturers do not tackle, under the spirit of 'San-so.' The value of the Yamato Kasei Group lies in launching new products into the world through original technology development that does not imitate others. With this sentiment in mind, we adopted "We are Chemical Innovators" as our corporate slogan. To put this slogan into practice, we will continuously challenge ourselves with new, interesting, and unprecedented endeavors.