(Sludge Recovery) Successful Case 1 (The cutting fluid life of the casting machining center has doubled!)

サノテック
1. Background of Introduction - In the case of cast iron cutting, the chips are fine and contain a large amount of carbon, leading to frequent troubles caused by clogging of high-pressure pumps and nozzles... 2. Effects After Introduction - As a result of a two-month test, the lifespan of the cutting fluid was extended to twice its original duration, and the defect rate showed astonishing results... ★ For more details, please be sure to check the "Case Study Materials"! ☆ We can provide proposals based on usage conditions and installation environments in collaboration with the manufacturer.