What causes parts to warp when heated? Measures against thermal deformation of thin plates.
When I took it out of the oven, the plate was warped. I will explain how to suppress thermal deformation caused by the difference in heating and cooling speeds.
last updated
-

What causes paint to string? Viscosity and solvent balance.
Paint stretches and adheres like threads from the gun. The stringing is stopped by the viscosity and the evaporation rate of the solvent.
last updated
-

What is the cause of the thin area around the hole? Static electricity and film thickness distribution.
The film thickness gauge is acceptable, but the coating is thin only around the hanging hole. I will explain the relationship between the escape path of static electricity and posture.
last updated
-

What causes fingerprints to remain on the paint? Barehanded work and oil residue.
Even though I painted it neatly, the shape of my fingers is showing through. I will explain the mechanism of how the oil from the hands repels the paint film and the management of gloves.
last updated
-

What is the reason for the uncertainty in the painting delivery schedule? Waiting for the batch in the curing oven.
Although the quantity is small, the delivery time is long. The cause lies in the batch unit of the baking furnace and the setup for color changes.
last updated
-

What is the reason for the difference in painting estimates between companies? The difference in the number of pre-treatment processes.
The estimates differ by double on the same drawing. The cause of the difference is not the paint, but the number of pre-treatment processes. Here’s an explanation of the perspective for comparison.
last updated
-

What are the reasons for the inability to read the costs of repainting? The cost structure of repainting.
The loss of one defective item is not just the cost of painting. We will break down the true cost, including stripping and re-preparation.
last updated
-

What causes lumps in paint? Management of usable time and storage temperature.
Bumps appear on the blown surface. It may not be a foreign substance but rather the gelation of the paint. I will explain the storage conditions.
last updated
-

What causes color changes in a batch? Mixing and baking time.
Even though the paint is the same and has the same color number, the color differs between batches. I will explain the effects of insufficient mixing and differences in curing time.
last updated
-

What causes residue from masking adhesive? Heat-resistant tape and removal timing.
When the tape is removed, the adhesive remains burned on. This explains the procedure to prevent adhesive residue based on heat resistance temperature and peeling timing.
last updated
-

What are the causes of powder coating not adhering? Grounding issues and jig management.
Despite the same conditions, only some products do not have powder on them. I will explain the grounding resistance of electrostatic coating and the dirt on the fixtures.
last updated
-

What causes rust at the corners of Bali? Edge coating and chamfer management.
The surface is intact, yet only the corners of the cut surface are rusting. I will explain the key points of edge rust prevention based on the relationship between burrs and film thickness.
last updated
-

What causes the painted surface to stick? Cooling management to prevent stacking marks.
When I opened the package, the painted surfaces were stuck together. I will explain the cooling time and loading conditions to prevent blocking issues.
last updated
-

What is the cause of paint peeling only at the welded areas? Residual scale.
The base material is unharmed, but only the area around the bead has the paint film lifting. We will stop the peeling of the weld area with the removal procedure for spatter and scale.
last updated
-

What causes the smell of paint to linger? Management of residual solvents.
Although it feels dry to the touch, the solvent smell doesn't go away. I will explain the management points to detect internal moisture that hasn't dried.
last updated
-

What causes white stains to remain after drying? Measures against water stains.
White ring stains left after cleaning. This explains how to prevent them before painting by managing water quality and drying time.
last updated
-

What causes the coating to be scratched by nails? Insufficient hardness and burn-in.
The paint film is scratched by nails after delivery. The cause lies not in the performance of the paint, but in the curing temperature and time.
last updated
-

What causes bleeding at the masking edge? Basics of application.
The bleeding and burrs at the edges are not due to the quality of the tape. They are determined by how it is applied and when it is removed.
last updated
-

What are the causes of scratches on the painted surface? Three points: transportation and fixtures.
Scratches occur not during the painting process, but during transportation and with fixtures. I will explain three measures that include packaging.
last updated
-

What causes the substrate to be transparent? Poor concealment and film thickness design.
The transparency of red and yellow is not solely due to the lack of hiding power in the paint. We will reconsider the undercoating design and film thickness.
last updated
-

What causes variations in film thickness? Three basic points for measurement and management.
Variations in film thickness are not due to differences in skill. This explanation will cover management methods that reconsider measurement points, jigs, and positions within the furnace.
last updated
-

What causes paint film to crack? Three conditions to prevent cracking.
The paint film cracks due to bending and temperature changes. Thickening and over-baking take away flexibility. It can be prevented by optimizing film thickness and baking conditions.
last updated
-

What is the reason for the inability to coat recesses in powder coating? The barrier of static electricity.
Only the inner sides of the box and the bottoms of the deep ribs do not have a film thickness. I will explain the Faraday cage phenomenon that prevents static electricity from entering and the countermeasures.
last updated
-

What causes the peeling of layered paint? The three barriers to interlayer adhesion.
The base is fine, but only the repaired layer is peeling off. The hardened paint film does not adhere. Surface preparation and time management will be the turning point.
last updated
-

What are the causes of color mismatch? Three basics of color difference management in painting.
The color does not match the previous lot and adjacent parts. The cause is the film thickness and baking temperature. I will explain a method to manage this with numerical values instead of visual inspection.
last updated
-

What causes paint to turn white? Humidity management to prevent whitening.
White discoloration that occurs frequently during the rainy season and summer. It is a phenomenon where the paint surface cools and condenses due to the evaporation of the solvent. It can be prevented by selecting the right thinner and managing humidity.
last updated
-

What causes marks to remain on the paint? Three methods to prevent fixture marks when hanging.
Hanger marks, gripping marks, exposed substrate. By specifying the contact position of the jig and managing conductivity, appearance defects and rework labor can be significantly reduced.
last updated
-

What causes the corners to rust first? The pitfalls of edge film thickness.
The flat surface has no issues, but the corners are rusting. The film thickness at the edges drops to less than half of that on the flat surface. We will improve this by requesting a chamfer and adding measurement points.
last updated
-

What causes bubbles in the coating? Drying management to prevent defects.
Countless small bubbles that appear after firing. The occurrence of pits caused by trapped solvent can be prevented by adjusting the setting time and heating rate.
last updated
-

What causes a rough painted surface? Three basics to prevent citrus peel skin.
Yuzu skin undulates like the peel of a mandarin orange. Smoothness is stabilized by three conditions: viscosity, film thickness, and gun distance, along with seasonal thinner selection.